Products
Irradiated Cross-linked Cable Compound
Description
This product is made from the basic material of polyolefin resin with the addition of high-quality and efficient halogen-free flame retardant, cross-linking agent and other processing additives by mixing, smelting, plasticizing and pelleting. The product is provided with not only excellent mechanical and physical properties , electrical properties, flame retardancy and processing performance but also non-halogen containing and low smoke, and is applicable for power cables, control cables, shipboard cables, optical cables, signal cables and so on.
Typical Values of Main Property
Performance |
Unit |
Typical Value |
|
Tensile Strength |
Mpa |
11.5 |
|
Elongation at Break |
% |
220 |
|
Thermal Aging |
℃×h |
136×168 |
|
Tensile Strength Retention Rate |
% |
95 |
|
Retention Rate of Elongation at Break |
% |
88 |
|
Volume Resistivity at 20℃ |
Ω*cm |
5.0×1014 |
|
Dielectric Strength |
KV/M |
26 |
|
Oxygen Index |
% |
33 |
|
Smoke Density |
With flame |
|
64 |
Flameless |
|
135 |
|
Ph Value |
|
5.7 |
|
Electrical Conductivity |
µ s/cm |
1.1 |
|
Low-temperature Embrittlement Temperature |
℃ |
-42 |
|
Thermal Elongation Test |
|
200℃×15min0.2Mpa |
|
Elongation under Load |
% |
58 |
|
Permanent Deformation after Cooling |
% |
1 |
|
Cable Combustion Flammability |
- |
Flame retardant class B |
Irradiation Dose: the recommended dose is 12-15MRAD.
Packaging
Two-layer moisture-proof package: film bag for inner layer and kraft paper bag for outer layer (or customer-specific package). The net weight of each bag is 25Kg.
Transporting and Storing
(1) Shelf Life: three months
(2) Put in a dry and cool place
(3) Avoid direct sunlight or rain
(4) Forbid broken package